Sikora inspection and measuring systems ensure the HV and EHV cables
HV and EHV cables place the highest demands on their function and their production. As submarine and underground cables, they ensure that electricity is reliably transported to where it is needed. A recent report identifies cable failures as one of the biggest challenges for offshore wind power in the future and predicts about 3,600 cable failures between 2024 and 2035, which could potentially cause costs of around 61.5 billion euros . This makes it even more important to ensure the quality of these cable types at the highest level.
For this reason, cable manufacturers rely on the latest inspection and measuring technologies from SIKORA, which monitor the plastic material for the insulation as well as the cable dimensions at crucial positions in the CV lines.
The purer the XLPE material used, the lower the risk of cable breakdown and the higher the life expectancy of the cable. In particular, when manufacturing long cable lengths, manufacturers aim at using as few cable connectors (joints) as possible, which is why material purity plays a crucial role. In addition to using melt screens after the extruder, the testing and sorting of the pellets before extrusion is of central importance.
The PURITY SCANNER ADVANCED ensures seamless inspection: it inspects 100 % of the material for purity already before extrusion and automatically removes contaminated pellets, for example those with metallic impurities from 50 μm. This ensures that only high-quality, pure material enters the extruder.
ULTRATEMP 6000 |
Another crucial factor is the melt temperature of the XLPE material during extrusion. The right temperature ensures a homogeneous polymer melt and prevents premature cross-linking. This is where the ULTRATEMP 6000, which is used in the flow channel between the extruder and crosshead, plays a central role. It continuously measures the melt temperature, thus ensuring an optimum temperature and enabling an optimization in extruder output of up to 15 %. In addition, a CV line has to be stopped after a certain production time to clean the extruder, screens and extrusion tools. Due to the optimized output of the ULTRATEMP 6000, the production length can be increased by up to 115 % before cleaning is necessary. This not only leads to higher efficiency, but also reduces the number of cable joints – which optimizes both cable quality and costs.
Directly after the crosshead, another SIKORA system is used: the X-RAY 8000 ADVANCED X-ray measuring system precisely records the dimensions of the cable, including wall thickness, eccentricity, diameter and ovality, directly in the CV tube. Visualized in real time, the measured values enable quick centering of the extrusion tools and distortion-free control to the nominal dimension. At the end of the CV line, the X-RAY 8700 NXT measuring system also ensures precise measurement of the “cold values” of the cable. In combination with the X-RAY 8000 ADVANCED at the beginning of the line, the shrinkage values for all three insulation layers of the cable can be precisely determined. Furthermore, the operator is shown whether the eccentricities of the individual layers and the ovality between the hot and cold measuring points have changed, which is an important information during the cross-linking process in the CV tube.
LM SMART |
Finally, the LM SMART length measurement system at the end of the CV line ensures that the required cable length is precisely maintained – a further contribution to quality assurance and resource conservation.
The intelligent integration of inspection and measuring systems along the entire CV line ensures the continuous quality of HV and EHV cables. From material purity and optimum melt temperature to precise monitoring of cable dimensions: A comprehensive quality approach ensures maximum reliability, safety and cost efficiency – all of which are indispensable for modern energy infrastructures.